Meegan Posted September 24, 2023 Report Share Posted September 24, 2023 Hi! I was Bisque firing my low-fire clay body to Cone 06 in my L&L Electric kiln and it konked out. Pretty sure it made it to 1300 degrees out of the desired 1828 degrees I usually Bisque to Cone 06, glaze it and then Glaze fire to Cone 06. Should I re-fire to Cone 06 before glazing? Or do we think it's ok to glaze and then just re-fire to Cone 06? Thanks! Quote Link to comment Share on other sites More sharing options...
Min Posted September 24, 2023 Report Share Posted September 24, 2023 I'ld do it again to your usual cone once you have your kiln sorted out. Hulk 1 Quote Link to comment Share on other sites More sharing options...
Kelly in AK Posted September 25, 2023 Report Share Posted September 25, 2023 You run a higher risk of having blisters or pinholes unless you re-bisque to the temperature you know works. Hulk 1 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.