Kelly Posted March 8, 2013 Report Share Posted March 8, 2013 Hi I've found some old glaze (nearly 5 years old) and I've opened the lid and it hasn't evaporated, but I can see under the water that there is a green mould on top of the settled ingredients. Am I right to presume the glaze should be thrown away? Link to comment Share on other sites More sharing options...
neilestrick Posted March 8, 2013 Report Share Posted March 8, 2013 The mold will burn out. Mix it up with a stick blender and use it. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted March 8, 2013 Report Share Posted March 8, 2013 You could put a few drops of bleach or peroxide in it and stir it up. Leave the lid off to let the peroxice or bleach evaporate out. Should be fine. Marcia Link to comment Share on other sites More sharing options...
Kelly Posted March 8, 2013 Author Report Share Posted March 8, 2013 Many thanks to you both, I really appreciate such prompt replies Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.