mrcasey Posted March 4, 2023 Report Share Posted March 4, 2023 This pot was made with white mid-range stone ware: Laguna #65. It was fired once, but some of the glaze crawled, so it was reglazed and fired again. There was a clean horizontal break all the way around. The pot was slab constructed and the walls are convex. Does anyone know what might cause this? Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted March 4, 2023 Report Share Posted March 4, 2023 I wouldn’t over think it. Refires are hard on pots as virtually all fluxed reactions have already occurred in the first firing, except for the new applied glaze of course. My expectations for refires are low and if I can downfire then my chances of survival are better in my experience. mrcasey and Rae Reich 2 Quote Link to comment Share on other sites More sharing options...