This pot was made with white mid-range stone ware:  Laguna #65.  It was fired once, but some of the glaze crawled, so it was reglazed and fired 

again.  There was a clean horizontal break all the way around.  The pot was slab constructed and the walls are convex. 

Does anyone know what might cause this?  

 

May be an image of indoor

Link to comment
Share on other sites

I wouldn’t over think it. Refires are hard on pots as virtually all fluxed reactions have already occurred in the first firing, except for the new applied glaze of course. My expectations for refires are low and if I can downfire then my chances of survival are better in my experience.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.