Kiln technician help neede Posted October 26, 2022 Report Share Posted October 26, 2022 How do you start a used Duncan Teacher Plus kiln? It will not reach temperature. Quote Link to comment Share on other sites More sharing options...
Kiln technician help neede Posted October 27, 2022 Author Report Share Posted October 27, 2022 How do you get a Duncan Teacher Plus Kiln up to temperature ? Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted October 27, 2022 Report Share Posted October 27, 2022 (edited) It sounds as if you have started the kiln and need to troubleshoot. To that Duncan made this general manual https://aakilns.com.au/pdf/Duncan_Kiln_Service_Manual.pdf which covers some of the the how to for their kilns in general. Can you tell us a bit about the model, model #, wattage, voltage, picture of the equipment tag, how it’s currently wired such as size breaker, etc….. and anything else such as if you know all the elements are glowing ….. post a picture if possible, I think that will help folks to ask questions or make suggestions. operation manual here if you do not have it : https://paragonweb.com/wp-content/uploads/LX851_Duncan_Energy_Saver_Owner_Manual.pdf Edited October 27, 2022 by Bill Kielb Quote Link to comment Share on other sites More sharing options...
neilestrick Posted October 27, 2022 Report Share Posted October 27, 2022 On 10/26/2022 at 1:43 PM, Kiln technician help neede said: How do you start a used Duncan Teacher Plus kiln? It will not reach temperature. Check out THIS THREAD. Lots of good Duncan info. Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.