mika Posted April 19, 2022 Report Share Posted April 19, 2022 I forgot about my green ware for two months... Finally I found some motivation to glaze it, but totally forgot about bisque firing... Do you think it will explode in the kiln? What do you think will be the outcome? It's a mug for a friend. I am very new when it comes to pottery... I feel so defeated because I spent so much time painting every detail on the mug Link to comment Share on other sites More sharing options...
Mark C. Posted April 20, 2022 Report Share Posted April 20, 2022 It must fire up very slowly at first like a bisque fire-No telling the outcome Go for it let it get very dry again 1st welcome to the forum Link to comment Share on other sites More sharing options...