laughlin Posted October 7, 2021 Report Share Posted October 7, 2021 Hm, I know I can use Velvet UGS on bisqued clay, but can I layer them onto bisqued underglaze? I want to do touch ups on the bisqued piece before glaze firing. (I figure I should bisque again if that's something that I can do so that nothing runs as it's a lot of teeny detail.) Thanks! (Tried to post this question yesterday but it's not showing up, sorry if it's a double.) Link to comment Share on other sites More sharing options...
Min Posted October 7, 2021 Report Share Posted October 7, 2021 Yes you can do this. Un-bisqued area might not take up quite as much glaze but not something I'ld worry about. Make sure the un-bisqued underglaze is really dry before glazing so it doesn't smudge. Link to comment Share on other sites More sharing options...
laughlin Posted October 8, 2021 Author Report Share Posted October 8, 2021 Thank you! (Hugely) Link to comment Share on other sites More sharing options...