ashhorth Posted August 25, 2021 Report Share Posted August 25, 2021 Can stonecast powder be fired in a kiln? It’s like a concrete ? thanks Link to comment Share on other sites More sharing options...
Bill Kielb Posted August 25, 2021 Report Share Posted August 25, 2021 I don’t believe they generally can withstand more that 650c . Many ceramic kilns with a controller can be fired to any temperature to about 1200c, what are you trying to do? Link to comment Share on other sites More sharing options...