Diane Howell Posted July 30, 2021 Report Share Posted July 30, 2021 Help! I sat a pot on 3 kiln shelf supports thinking I would keep it from sticking to the kiln shelf. It didn’t stick to the shelf but the glaze attached one of the kiln supports to the pot. What can I do??? Could I retire the pot and elevate it more than the support and hope the support falls off during firing? I’ve tried tapping and nothing has happened. Any suggestions? Link to comment Share on other sites More sharing options...
oldlady Posted July 30, 2021 Report Share Posted July 30, 2021 assuming your clay an earthenware so that stilts are necessary? grinding it off with a tool, dremel hand held or standing grinder depending on the size of the blemish. then you still have the decision about refiring. maybe it would be better to make a new one depending on the complexity of the pot decoration and your available time and interest in saving it. saving errors is also educational. Link to comment Share on other sites More sharing options...
Chilly Posted August 1, 2021 Report Share Posted August 1, 2021 Try popping it in the freezer for 24 hours. The GENTLY tap the post while holding the pot. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.