Mark C. Posted May 22, 2021 Report Share Posted May 22, 2021 Been lots of luster questions lately The best practice is to test lusters they work best on smooth surfaces Long ago when I did lots of luster work I took a test piece and ran all my luster tests on that so I could see what they actually look like I suggest this to anyone who is starting with lusters-these days you choices are very limited but as you can see by this test pice in the early 80s they made lots of colors back then This test was on a low fire clear that loved to craze on a refire but it shows the colors and a list is always a good idea to back up the test. I have many tests like this with glazes or pencils or slips-whatever-testing keeps you from making lots of mistakes even though with testing mistakes will still happen as its part of ceramics Link to comment Share on other sites More sharing options...