Marina101 Posted May 22, 2021 Report Share Posted May 22, 2021 Hi, I have terracolor glazes, both in powder and fluid. My question is if you have tried layering them, like you would do with amaco for example. And If you can layer the powder with the fluid. If you have any other info about coat thickness or difference of application feel free to share. Link to comment Share on other sites More sharing options...
Chilly Posted May 22, 2021 Report Share Posted May 22, 2021 When I buy/make new glazes I always do some test tiles. For layering, I make an L shape, so some is vertical and some horizontal I apply a stripe of each glaze in one direction, then apply a stripe of each (keeping the same sequence) in the opposite direction. Do this on both vertical and horizontal surfaces That gives a reference as to how nicely, or not, they play together. Remember every glaze will be different on your clay to mine, in your kiln to mine, and in the way we each apply the glazes. Have fun. I often spend more time on test tiles, than on making real stuff. Link to comment Share on other sites More sharing options...
Marina101 Posted May 22, 2021 Author Report Share Posted May 22, 2021 Thanks for the advice! Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.