Thisislin Posted February 3, 2021 Report Share Posted February 3, 2021 Hi there, I have this vase with what I assume is some kind of reactive glaze, my knowledge of glazes is effectively zero at the moment. I just can’t find any examples or recipe for what it. It looks like lots of bubbles and the most similar I can find are chunky volcano glazes. It’s hard to tell in the photo but it’s very textured, the bubble outlines are raised but it has a slight iridescent shine at the same time. Does anyone know what this is called so I can do further research or have any related information? It’s much appreciated. Thank you!! Sample of Glaze Sample of Glaze 2 Link to comment Share on other sites More sharing options...
Min Posted February 3, 2021 Report Share Posted February 3, 2021 Do a search on Glazy using the terms Lava, Crater and Silicon Carbide. It's going to take a fair bit of testing getting that surface quality. Here's one example from there. https://glazy.org/recipes/110904 Welcome to the forum. Link to comment Share on other sites More sharing options...
Thisislin Posted February 7, 2021 Author Report Share Posted February 7, 2021 Thank you, I’ll look into those! Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.