Lucy GReen Posted January 2, 2021 Report Share Posted January 2, 2021 Does anyone have anyyy idea how I'd make such a beautiful glaze. I'm in love with it and I've been searching for hours but adding frit to a glaze/ crystalline glazes don't have quite the same appearance and I'm pretty sure it isn't just a splatter glaze. Thanks to anyone that can help! Link to comment Share on other sites More sharing options...
neilestrick Posted January 2, 2021 Report Share Posted January 2, 2021 It's either a mojolica type apllication, where saturated colors are put on top of a white base glaze, or it's simply underglazes with a clear over the top, on white clay. Link to comment Share on other sites More sharing options...
Min Posted January 2, 2021 Report Share Posted January 2, 2021 Looks a fair bit like the Mayco Jungle Gems. (image from their website) Link to comment Share on other sites More sharing options...