BonnieBee Posted December 17, 2020 Report Share Posted December 17, 2020 Why would some of my bowls break, during glaze firing, on one side of the foot? I use wax resist on the foot and base. This has happened way to often recently. Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted December 17, 2020 Report Share Posted December 17, 2020 Hi Bonnie! Theres a lot of reasons it could be happening. Do you happen to have a picture on your phone you can upload? Barring that, could you describe what kind of clay you’re using, how thick the pieces are, the glaze you’re having issues with, how it’s been applied, the recipe if possible and the firing cycles? Link to comment Share on other sites More sharing options...