OlgaR Posted November 30, 2020 Report Share Posted November 30, 2020 Hi guys, I added too much water to my glaze. Would it make any harm if I boil it a little to evaporate the excessive water? Link to comment Share on other sites More sharing options...
akilspots Posted November 30, 2020 Report Share Posted November 30, 2020 boil the glaze? i think you would be better off letting it settle for a day or so and trying to siphon off some of the water. problem is some of the glaze recipe ingredients might be water soluble. probably best to add some dry mix to the wet. Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted November 30, 2020 Report Share Posted November 30, 2020 +1 for adding a little dry mix. Link to comment Share on other sites More sharing options...