V__ Posted November 17, 2020 Report Share Posted November 17, 2020 Hi, I just unloaded a glaze fire and unfortunately all of my pieces have pinholes in them :( Please help, what causes this and how can I avoid this for happening again. Can I fire again and hope that it solves the problem? Thank you in advance for the help! Link to comment Share on other sites More sharing options...
liambesaw Posted November 18, 2020 Report Share Posted November 18, 2020 What clay body, what glaze Link to comment Share on other sites More sharing options...
Bill Kielb Posted November 18, 2020 Report Share Posted November 18, 2020 1 hour ago, V__ said: Can I fire again and hope that it solves the problem? Lots of causes for pinholes and sometimes difficult to cure . Pictures, more info. The more the merrier. Clay, glaze, cone for each, cone it was fired to, schedule it was fired at............ and refining will most likely not fix your pinholes. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.