Sorcery Posted November 12, 2020 Report Share Posted November 12, 2020 On 11/10/2020 at 1:30 PM, Rick Wise said: I have concluded to my own satisfaction that I got a bad batch of clay from Standard. After changing clays all the problems disappeared as quickly and as mysteriously as they had arrived. I also noticed that the un-used clay in the bag had, after sitting a while, begun to develop fissures in it. Weird -- but glad to know this is possible. Would you happen to have the box still? It would be good for the community to report the batch to your supplier and Standard, so it can be noted and recalled. Sorry to hear that, but glad you're better! Sorce Link to comment Share on other sites More sharing options...