In general, brushing on top of a dipping glaze can be difficult. Because the dipping glaze doesn't have the hardeners and binders in it, you may find that the brush picks up the dipped glaze  rather than just going over the top of it. It will depend on the makeup of the glaze. Those with higher clay content will probably work better. I would also do the brushing glaze before the dipped glaze is totally dry. If glazes can have a leather hard stage, that would be the time to do it. Like when it's dry enough to touch but not totally bone dry.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.


×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.