Jump to content
Sign in to follow this  
cf66

Substitute for Fusion frits F-524 and F-69

Recommended Posts

I'm in Europe and can't find them at all, help!!

I even called Aardvark Clay, my sorely missed supplier in the greater Los Angeles CA area, and even they don't have them! I've also contacted Scarva and Potterycrafts in the UK, nada either.

It's for this recipe (published on Digitalfire.com):

Cone 04 UltraClear Glossy Base

Code: G3879
Modification Date: 2019-07-19 14:54:26

Material Amount Percent
Fusion Frit F-524 850.0 82.9%
Fusion Frit F-69 40.0 3.9%
EPK 90.0 8.8%
Silica 45.0 4.4%
  1025.00  

Any ideas?

Thanks in advance.

Share this post


Link to post
Share on other sites

Time to bust out your glaze calculator!

 

Looks like mostly a low expansion barium strontium frit.  Yikes!  Will definitely want to use frits to reformulate, I just don't know what frits are available in Europe.

Or just use a different recipe with readily accessible ingredients

Edited by liambesaw

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.