LineByEva Posted August 25, 2019 Report Share Posted August 25, 2019 Title says it all, I made a mistake, can I re-fire at the proper cone 6 temputure and pull off a save? What's your thoughts? Eva Link to comment Share on other sites More sharing options...
Denice Posted August 25, 2019 Report Share Posted August 25, 2019 Yes you can refire to C6, I can't promise it will fix your glaze. Most C6 glazes will fire at C5, what is the problem with your glaze? Some glazes do not like to be refired and it might make it worse. Denice Link to comment Share on other sites More sharing options...
neilestrick Posted August 27, 2019 Report Share Posted August 27, 2019 It may or may not look the same. Also, because the glaze has already been melted once, it will melt a little easier the second time, so it will probably be a little runnier than if you had fired to to cone 6 once. Link to comment Share on other sites More sharing options...