MollyMac Posted March 24, 2019 Report Share Posted March 24, 2019 Ideas? Love this effect. Slip/underglaze/oxides ??? I am still a beginner sculptor, a real glaze beginner, but I want to head toward this idea! Link to comment Share on other sites More sharing options...
Min Posted March 24, 2019 Report Share Posted March 24, 2019 Veronica Cay piece for which she says she used terra cotta clay with underglazes, engobes and stains. It's going to take some experimenting with brushing on then wiping off, building up layers etc. Link to comment Share on other sites More sharing options...