potteryteach Posted October 28, 2018 Report Share Posted October 28, 2018 Can anyone help me with how to make a black iron oxide wash recipe? And phrase it for the layperson? I don't understand how to read ceramic glaze recipes. I'm a little out of my element. Thanks! Link to comment Share on other sites More sharing options...
neilestrick Posted October 28, 2018 Report Share Posted October 28, 2018 What cone are you firing to? If you don't want to mess with mixing your own, just water down a commercial underglaze. Link to comment Share on other sites More sharing options...
potteryteach Posted October 28, 2018 Author Report Share Posted October 28, 2018 Firing to Cone 6 Link to comment Share on other sites More sharing options...
liambesaw Posted October 29, 2018 Report Share Posted October 29, 2018 For washes you can use oxide + water. For something with a little nicer result, oxide + frit + water. For something good for brushwork, oxide + glycerin Link to comment Share on other sites More sharing options...
potteryteach Posted October 30, 2018 Author Report Share Posted October 30, 2018 Thank you so much! Link to comment Share on other sites More sharing options...