Cherry Posted October 29, 2017 Report Share Posted October 29, 2017 My chemistry background is basic but every time I siphon water from a runny glaze or slip, I wonder- Am I changing the chemical make-up an appreciable amount because of solubles I'm removing ? What solubles are there? Am I overthinking this? Link to comment Share on other sites More sharing options...
Marcia Selsor Posted October 29, 2017 Report Share Posted October 29, 2017 this is a good article from Digitalfire regarding water soluble glaze chemicals https://digitalfire.com/4sight/glossary/glossary_water_solubility.html You are not over thinking it. Marcia Link to comment Share on other sites More sharing options...
Cherry Posted October 29, 2017 Author Report Share Posted October 29, 2017 Thanks, the article is great. Link to comment Share on other sites More sharing options...