windingpathpottery Posted October 21, 2017 Report Share Posted October 21, 2017 Looking to make a clear glaze for Cassius Basaltic body to fire at cone 5 in electric kiln. My present clear glaze is Hesselberth & Roy High Calcium Semimatte Base 1, which is perfect on everything but Cassius. Any help is greatly appreciated. Link to comment Share on other sites More sharing options...
neilestrick Posted October 21, 2017 Report Share Posted October 21, 2017 In what way is it not working? Link to comment Share on other sites More sharing options...
kristinanoel Posted January 16, 2018 Report Share Posted January 16, 2018 Hi Winding Path Pottery - did you ever find a clear glaze recipe that works? I just got some cassius black to play with, and want a clear, white, or white matte for it if you found one! Link to comment Share on other sites More sharing options...