Babs Posted April 29, 2019 Report Share Posted April 29, 2019 Saucers fired inHotter area of kiln? Bubbles..maybe fettle the glaze prefiring for any blemishes. Saucers bubbled? If not, maybe add a short soak at end of firing. Medals for suc h perseverance:-) Link to comment Share on other sites More sharing options...
njabeid Posted April 29, 2019 Author Report Share Posted April 29, 2019 If the saucers had been hotter, they would have been glossier ... is that so? They were alone at the bottom, actually maybe a wee bit cooler. Good point. Not bubbled, they are lovely and I love the contrast. I thought they would be the same colour as the stencilled patterns, but those got covered up. Only the bowl has about five small burst bubbles on the inside. 15' soak. Thanks for the medals! I'll get there one day. Link to comment Share on other sites More sharing options...