Have small quantities of chemicals I inherited and need glaze recipes for cone 6.

These are the chemicals: red iron oxide, rutile frit, manganese carbonate, copper carbonate, cobalt carbonate, nickel carbonate, borax, feldspar custer, zinc oxide, bone ash, chrome oxide, albany slip and barnard blackbird slip.

What main ingredients are missing to make glazes?

Where can I find recipes to make best use of these chemicals?

Link to post
Share on other sites

You have mostly colorants except for the borax, bone ash, and custer feldspar. If you are doing ^6 oxidation , you may need more fluxes like Dolomite, Nepheline Syenite, Gertsley Borate or a substitute, and the basic clays like Kaolin,Silica,ball Clay.

The best books for mod-range glaze recipes and understanding how things work are:

Mastering ^6 Glazes by John Hesselberth and Ron Roy

^6 Glazes by Michael Bailey

Mid Range Glazes by Jphn Britt

 

Marcia

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.