g-bus Posted April 27, 2016 Report Share Posted April 27, 2016 So after pestering you fine folks about rehabilitating on old Skutt 1027 I decided that I really didn't want to put a bunch of time and money into an old kiln that is not in the best shape, and instead am having a kiln rebuilt for me by a semi-local L&L distributer. It's basically a J230 with new electronics and elements, however it has a manual controller. I really want to go with an electronic controller and apparently to retrofit this one with a hardwired version was not really going to be cost-effective so am looking at wall-mount/plug-in styles. From my research it looks like my options would be something like the Skutt wall-mount Kilnmasters, an Orton Autofire, or a Rampmaster for the plug-in styles. And then there's the Electro Sitter, which from what I can determine looks like is a unit that replaces the kiln sitter, and then has the option of going with a few different control panels, of which the Bartlett V6-CF seems to be a pretty solid choice. I do really like the idea of the Genesis, but haven't found that as an option, so would require buying an Electro Sitter with a different control board and then replacing it with the Genesis, but that would be really expensive and kind of a waste for just a little bling on my kiln. Oh yeah, and then there are all those cheap controllers on eBay for under $100, and while I'm sure some are OK for certain uses, I'm pretty skeptical. So, I'm asking for some input and suggestions as to what would be a good option for me (just a hobbyist, not a production potter......yet). Obviously keeping the cost lower is better, but I want something quality that will be reliable and last a while, and that I won't outgrow in a year (even though I know I could get by with just a kiln sitter indefinitely). I'm comfortable doing some light electrical work if need be. Ok, one last thing, should I consider something that will control all three zones independently or just stick with a controller with one pyrometer? Having something that could adjust each zone independently sounds pretty cool, but from what I've read sounds like it can put a bit of extra strain on elements and relays. And if I really had issues with cold spots couldn't I potentially compensate for this by just adjusting the infinite switches, thereby eliminating the need for a 3-zone controller? Thanks so much for your help! Link to comment Share on other sites More sharing options...
ronfire Posted April 27, 2016 Report Share Posted April 27, 2016 I am thinking of the same for my Skutt 1027. Have not decided on what route to go with but am leaning on using a genesis with zone control. This does not look difficult to remove the sitter, wire in 3 thermocouplers, 3 relays and a centre tap transformer. My biggest thing I need to find out is mounting the thermocouples . There are several wiring diagrams available how to wire the controller. If I do not use zone control I would then go with a wall mount system and leave the sitter on the Kiln. Link to comment Share on other sites More sharing options...
neilestrick Posted April 27, 2016 Report Share Posted April 27, 2016 Any of those options would work, with the exception of the eBay versions. While they would probably work, the controllers made specifically for kilns are a lot more user friendly and do the cone calculations for you. Any kiln company that uses Bartlett controllers can also get the Genesis, so I would call them and ask what the cost difference would be. It's a direct swap with the V6-CF, so it should only be the difference in hardware costs. If you're going to this much trouble to rewire, and you really want the full benefit of a digital kiln, I would look into doing zone control. The Electro Sitter and other external controllers wouldn't work for that, though, since they use a single large relay. But, you could buy an empty control box from Skutt or L&L and build your own system for around $650, maybe less if you source the parts from the web. The L&L piggy-backed control box setup is the best, since the electronics stay cooler and they're easy to work in. Link to comment Share on other sites More sharing options...
g-bus Posted April 29, 2016 Author Report Share Posted April 29, 2016 Thanks for the info. That puts the L&L controller right in line with most of the others that I've been looking at in terms of price, but I assume it's quite a bit more involved as far as install goes, correct? If it's basically how Ronfire explained it then that's certainly within my realm of capability, just need to be sure I got all of the correct parts. Hmm, now you've got me thinking..... Link to comment Share on other sites More sharing options...
ronfire Posted April 29, 2016 Report Share Posted April 29, 2016 You can order all the parts from most Kiln supply shops. Relays thermocouple and a centre tap transformer. The control board might be able to order direct from Bartlet. Link to comment Share on other sites More sharing options...
neilestrick Posted April 30, 2016 Report Share Posted April 30, 2016 The only difference with the L&L is that there's a few more wires for the zone control, and more thermocouples. The L&L Dynatrol is the same thing as the Bartlett V6-CF, and the new Genesis has identical mounting and wiring. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.