Mark C. Posted May 11, 2017 Report Share Posted May 11, 2017 I think the anodizing would wear off pretty fast-same with epoxy but thats going to get into the clay as chunks. One other thought as mine is pitting and came pitted from low fire high school clay is live with it. You can have it bead blasted but why? When it wears out in a few decades replace it with a new one? Link to comment Share on other sites More sharing options...
Bryan Johnson Posted May 11, 2017 Report Share Posted May 11, 2017 I found the reaction of the aluminum with my clay formed hard nodules that would break off into the clay. Really messed up designs in colored clay. Link to comment Share on other sites More sharing options...