sparklingmango Posted June 6, 2015 Report Share Posted June 6, 2015 Hello all :-) Any tips, useful websites, etc for casting/making rings? I work with Egyptian faience and I would like to start making rings, but I don't know where to start from...Thanks :-) Link to comment Share on other sites More sharing options...
jrgpots Posted June 8, 2015 Report Share Posted June 8, 2015 1. would egyptian paste do well in an extruder? If so you could extrude tubes, then cut multiple rings from each tube. Each tube could be differt diameter corresponding to ring sizes. 2. Does egyptian paste shrink when fired? 3. If it does not do well in the extruder, could you spin cast it using a slurry of the paste? Jed Link to comment Share on other sites More sharing options...