ron Posted July 14, 2011 Report Share Posted July 14, 2011 On the southwest type pottery I see part dull black and part gloss black,how is this done,thanks Link to comment Share on other sites More sharing options...
Marcia Selsor Posted July 15, 2011 Report Share Posted July 15, 2011 The slip, similar to terra sig in that it is fine particles, is applied to the pot and burnished. Then more slip is painted on and not burnished, leaving a dull surface. Marcia Link to comment Share on other sites More sharing options...