Hi Bill,
You have been so helpful, I'm wondering if you could help me figure out my line for my kiln. Here are the specs.
BTUS x 1,000:
60
BTU/HR Total:
120,000
Gas Pipe Inside Dim:
3/4"
Propane (LP) Water Column Pressure:
11"
Natural Gas (NG) Water Column Pressure:
7"
No. of Burners:
2
Orifice Size Propane:
3/32
Orifice Size Natural Gas:
1/8
# of Gallons LP per Cone 10 Firing
5
I put my questions in all cap. The kiln is the olympic 18 inch torchbearer. I want to use a 20lb propane tank with a flexible line. From reading your above comments I gather I'll need a Qcc fitting handle (DO THEY COME IN ONES FOR 120,000 BTU?). Then a 1/4inch pigtail into a low pressure regulator (WHICH LOW PRESSURE REGULATOR?), THEN WHAT COMES OUT OF THE REGULATOR TO CONVERT TO 3/4INCH? I need a 3/4 in propane hose (HOW LONG AND DO YOU RECOMMEND THE ONE YOU RECOMMENDED ABOVE FOR MY KILN?) I will also need an on/off valve Because I don't have a safety ignition thing (DO YOU RECOMMEND A TYPE OF VALVE?)
THANKS SO MUCH, I live in a small town and can't find anyone to help.