Hi all,
I was wondering if anyone has used Imery's replacement for SSP, Kaopearl, in a successful slip? I've tried a variety of recipes, the last being this one which I used to use for SSP. There would always be slight adjustments but now the slip seems to be unable to take more deflocculant and I'm concerned about raising the water too high to keep the specific gravity in the correct range of about 1.75 -1.78
28l water
250 antiprex
450 alcosperse
35kg China clay (SSP)
25kg feldspar
11kg silica
Any thoughts would be appreciated.