Thank you all so much for your responses! I will try drilling it out somewhat to get it not entirely solid and then the slow re-wetting process and cross my fingers. If I lose it ultimately that's ok, but I really want to try.
Thanks again!
Jes
I made a sculpture last September and then had a bunch of things come up in life, as they do. I was just cleaning out my studio and found it again and it is bone dry, but way too thick to fire without a very high chance of exploding. Is there any hope of re-wetting the clay without destroying the sculpture?