This summer I purchased an older kiln at an estate sale. I’ve attached photos of the controls, and the model number. I’ve tried to fire to cone 04 a few times for a test firing, but so far the kiln sitter shuts off around 5 hours, and the self supporting cone is barely bent.
The top dial, I’m assuming is the temp, and the second a timer.
does anyone have any suggestions on a firing schedule? So far I’ve tried 2nd knob ON — 1st knob 4 hours at low, the switched to medium, and then the sitter shuts off after about an hour at medium.
any advice would be so greatly appreciated!!!! Thank you!!
Bridget