Hi, yes. I sent Joanna Oliver an email asking if she would share the recipe and she did. The only catch is the stain used is one sold in the U.K., not a Mason stain, so I have to figure that one out.
Hi n thanks. I’m confident I mixed it correctly, ha, but in the end I am going to make up another test batch to rule out any possibilities. I got the recipe from Britt’s book, under magnesium matte purples.
Why did my Pikes Purple come out green? The mix was spot on, but the sp gr was a paltry 139, instead of the recommended 160. This wouldn’t be the cause, would it?