Report How long is too long for Greenware in Clay and Glaze Chemistry Posted April 19, 2021 i had greenware sitting around for well over a decade. they survived a trip when i moved house and when i finally got the kiln plugged in, they fired perfectly as if i had made them only a week or so ago :-) Hulk 1
How long is too long for Greenware
in Clay and Glaze Chemistry
Posted
i had greenware sitting around for well over a decade. they survived a trip when i moved house and when i finally got the kiln plugged in, they fired perfectly as if i had made them only a week or so ago :-)