Jump to content

glazenerd

Members
  • Posts

    3,151
  • Joined

  • Last visited

4 Followers

Contact Methods

  • Website URL
    https://www.facebook.com/Clay-Tech-199305684284517/

Profile Information

  • Location
    St. Louis, Mo.
  • Interests
    Crystalline glaze chemistry. Porcelain, Stoneware, Fritware, 04 Colored Porcelain clay research & formulation.
    Ceramics Monthly Articles: Jan. 2018 Cation Exchange (plasticity), April 2018 SSA Clay Formulation, May 2018 Bloating and Coring.
    Feb. 2019 Ceramics Monthly- Clay Body Shopping Guide
    March 2019 Ceramics Monthly - Porcelain 201
    June 2019 Ceramics Monthly Clay Restoration
    Sept. 2019 Clay Memory
    Oct. 2019 Firing Programs

    Email: optix52@aol.com

Recent Profile Visitors

30,904 profile views

glazenerd's Achievements

Advanced Member

Advanced Member (3/3)

1.6k

Reputation

Single Status Update

See all updates by glazenerd

  1. So far I am really liking 75-104 utility porcelain. I formulated it to a specific set of limits in lieu of clay varieties. I can nearly pull up a bowl almost perfectly on the first pull. I pulled up a 4" x 10" cylinder with only one pound of clay. Think I will pug out 25 lbs here shortly, interesting properties indeed.

    1. glazenerd

      glazenerd

      Correction: 4" x 8" cylinder. The ten inch cylinders are from my translucent recipes.