Jump to content

glazenerd

Members
  • Posts

    3,267
  • Joined

  • Last visited

9 Followers

Contact Methods

  • Website URL
    https://www.facebook.com/Clay-Tech-199305684284517/

Profile Information

  • Location
    St. Louis, Mo.
  • Interests
    Crystalline glaze chemistry. Porcelain, Stoneware, Fritware, 04 Colored Porcelain clay research & formulation.
    Ceramics Monthly Articles: Jan. 2018 Cation Exchange (plasticity), April 2018 SSA Clay Formulation, May 2018 Bloating and Coring.
    Feb. 2019 Ceramics Monthly- Clay Body Shopping Guide
    March 2019 Ceramics Monthly - Porcelain 201
    June 2019 Ceramics Monthly Clay Restoration
    Sept. 2019 Clay Memory
    Oct. 2019 Firing Programs

    Email: optix52@aol.com

Recent Profile Visitors

33,826 profile views

glazenerd's Achievements

Advanced Member

Advanced Member (3/3)

1.8k

Reputation

Single Status Update

See all updates by glazenerd

  1. Threw some test cylinders from my high translucency formula this morning: much higher plasticity than any stoneware I have tried.

    1. Show previous comments  2 more
    2. glazenerd

      glazenerd

      Joseph: now that I have a clay body that is easy to throw- very well TY. I mixed up some of your Sio2 clay this morning.

    3. glazenerd

      glazenerd

      Joseph: by the way- the 6.18 COE does not hurt either- much easier to glaze fit.

    4. Joseph Fireborn

      Joseph Fireborn

      I imagine so. Good to hear your new clay is rocking.

×
×