I mixed 10lbs of Coma Clay, bisq yesterday. Pull them out of the kiln, slather some glaze on them, fire em up. First time to seriously test crystal results.
-
More SiC experiments or your old trusty glazes that you have shown on the new clay?
-
Crystalline glaze, but I did drop a ^6 red in ox in as well. Have to find the new hold ramp temp.
-
and?...