Single Status Update
-
my mugs were getting too dry to handle so I put them in my magic rehydration box. Now they are too wet to handle.
-
ugh not good- I use the zip lock tote boxes with a sealed lid.. I just mist a tad of water in them and my clay stays the same for literally months .. I guess you have potters plaster in yours?
-
So is your rehydration box the same as a wet box made with plaster? We had wet boxes at the college, but someone said that all the dried vessels put in there would not receive a handle without cracking around the handle. I've based my advice about rehydration
on their comments. :>( But thinking back 12 yrs., they did have sloppy techniques, which made our ideas clash.
-
No plaster. It's just an air tight Tupperware box I got from target.
-