  1. Back to the drawing board. I fired a kiln to ^6 with a pyro barin my sitter. New sitter, new everything, except infinite switches (no long can get), but it never got there. Brand new elements. It was firing fine till last nite. It's still cooling. Going to fire in my small kiln to finish an order. And work on the big kiln. I will fix it or try basket weaving in my padded room.

    1. glazenerd

      glazenerd

      It is not a set-back, just a new challenge.