Hi Callie, distributed by a french supplier CERADEL. The clay is GT5700B (to be fired between 1250°C and 1280°C). The glaze is "vert pré" EG225 (to be fired between 1180°C and 1250°C).
I fired à 1220°C.
-
Right, it was stoneware.
-
Yes I've built my ribbons. Someone told me to use clay grog (or with grog) and may be it should work. I'll try with different size of grog.
-
-
Hi, I've a problem. I made a piece with clay stoneware. When it dries = OK. When biscfire = OK. But when firing after glazing à 1220°C, the piece collapse, see pictures. Maybe the temperature is too high. But it's a long time I'm working this clay without problem. Whether I use earthware the piece doesn't collapse. But I want to use my glaze and I don't want to by glaze for earthware. What could I do ?
Thanks for advice
Sean
My pieces collapsed
in Clay and Glaze Chemistry
Posted
Thanks again for your comments, I'll see another shape or something else.
Keep you informed in case of success