So I got busy and made three sinks for a house I am renovating. This past week I loaded them up and bisque fired them. One of the three survived the bisque firing. The good thing is I know how to efficiently make two more. Must allow more drying time for 1/2 inch thick ware this time..
- Show previous comments 4 more
-
I need to make a couple of sinks someday. The ones in my bath are chipping. Denice
-
My friend made sinks and made a bowl to fire them in an upright position.
-
I have new clay for the remake of two sinks, it's a nice architectural clay , very groggy. This time I will take more time to dry, and punch some relief holes inside the foot ring near the foot/bowl join to let the water out better.