Roberta12 reacted to JohnnyK in 120621 kiln opening 1.jpg
This is a sample of my latest firing. The purple in the lids of the urns is apparently from the reflection of the wall behind the group. All glazes are Amaco Potter's Choice and Obsidian Celadon in layers fired to ^6. The mug in the front is actually a single firing (no bisque) which was successful. my next glaze firing will be a bunch of test tiles using the same glazes fired to ^5.
-
-