bisquekilnload.jpg
 
© yorkavenuestudio.com
Credit yorkavenuestudio.com

bisquekilnload.jpg



Very first batch of low fire clay pieces.  All loaded onto a 5X5 inch kiln shelf.  I have a Paragon SC2 kiln that I named Miss Piggy.  I use it often to anneal steel rods for making stamps and I fire metal clay silver and bronze.  

This first bisque firing was thrilling!  15 hours, very conservative ramp rate.  Like the first time trying to dress a newborn, I was being super careful.

 

Credit

yorkavenuestudio.com

Copyright

© yorkavenuestudio.com
From the album:

Beads Pendants Cabs Minis Low Fire Ceramics

  • 7 images
  • 0 comments
  • 0 image comments

Photo Information for bisquekilnload.jpg


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.