Joseph Fireborn 1,447 Posted April 27, 2017 Report Share They get more and more interesting each time. = ) Keep up the good work. Quote Link to comment
1515art 260 Posted April 28, 2017 Report Share Thanks Joseph, I've made a few of this type in the past and a customer just bought one I'd rakued a few years ago that some of the handle had broken during the firing. I only had two left and don't want to sell the other so she took the one with missing handle piece for $600 and wants to collect more work. Guess that means I should make a couple more in the series and see what happens? Quote Link to comment