Experimenting with bought tissue transfers and stencils as resist. Thrown white earthenware. Dipped in transparent glaze & fired to 1100oC in an electric kiln.

From the album:

2016

  • 6 images
  • 0 comments
  • 5 image comments

 Share


Recommended Comments

I love this Celia!  I see no signs of crawling either!   I am trying to wrap my head about the tissue transfers and the stencils.  You lay the stencil on the bowl and then apply the dampened tissue over it?

Link to comment

Yes that's about it Roberta. Stencils with the motif being the negative part (the holes). This one was actually some flower wrapping paper that was holey all over and I cut small pieces, laid them around the bowl, cut small pieces of tissue transfer paper, laid on top, sprayed lightly with water, rubbed them gently with a rubber tipped tool, left to dry then peeled off and removed the stencil.

The creamer stencil I made myself on a Silhouette stencil machine, cut from thin plastic film (thin filing wallets) as it's flexible enough for the curves. Same process. Lots of potential and given the price of stencils - quite a good use of them.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.