Wildflower Sponge Holder and Mug in Peach
Wheel thrown in buff stoneware with speckles. Carved with wildflowers and grass. Underglazed with Duncan Concepts Bright Kiwi. Interior glazed with Laguna Peach Blush. Flowers in Peach Blush, Dynasty Red, and Blackberry Wine. Exterior aside from flowers left raw.