Eucalyptus Carved Platter
White stoneware, thrown on the pottery wheel, carved in a design of eucalyptus leaves in the wind. Glazed in Mayco's Stoned Denim at ^6 in an electric kiln.
Copyright
© Giselle No. 5 Ceramics 2016, all rights reserved