Marko 191 Posted December 18, 2015 Report Share Nice. This is a first for me. I never heard of rice ash. But it has a beautiful effect. Good work. Quote Link to comment
Joe_L 76 Posted December 19, 2015 Report Share I think rice ash is high in silica. I forgot to say this was a reduction firing too. Quote Link to comment
glazenerd 1,807 Posted July 29, 2016 Report Share Love the granite look this firing produced- good job. Quote Link to comment
Joe_L 76 Posted October 4, 2016 Report Share Only just seen your comment Nerd, thanks. Don't know that much about the glazes, they're from a professional potter when I went on a course in his studio. The body is very iron rich. The blue glaze has a fairly high clay content, in his words almost a slip. The mottling on the white rice ash glaze is it interacting with the blue underneath it. Quote Link to comment